The first step: "sure"
Commonly used wood grain brick way of the shop is stuck, in addition to the traditional ceramic tiles as well shaped, horizontal flat vertical brick, wood grain brick and chevron, i-section, oblique ling line brick method.The shop is stuck way is varied, each has his strong point.So be sure to make sure the plan together with designers.
The second step: "leveling"
So-called leveling, immediately in front of the shop wood grain brick, deal with brick buildings floor or wall surface for processing.Such as floor, wall, external wall, etc.Eliminate surface attachments, with half wet water sediment mixture paving.
Step 3: "the play line"
Elastic line is refers to in a long, thin lines coated with white ink. The determine the central axis of brick, and then press the shop is stuck.
Step 4: choose "brick"
Brick shop to see whether the plan, the varieties, selected to classify.Such as floor of wood grain on the wood grain brick, wall brick, wood grain brick and so on to distinguish between the anchor line, lest paved mixed up.
Step 5: "immersed brick"
Wood grain brick is the same as polishing brick, and archaize brick to soaking water, to use tap water or water, cannot use water or dirty water, more can't oil wastewater;Soak time don't need too long time, that is to say, soaking wet.Soak (ceramics, must to the shop is stuck)
Step 6: "slurry"
Water and sediment should be mixed in a ratio of 1:2, should use the cement in the label is less than 200, high grade of cement to wood grain brick form should pull, severe cracking wood grain brick.
Step 7: "paste"
Remove soak good wood grain brick, dry wood grain brick stain, will apply evenly on the back of wood grain brick, cement mortar thickness in 2-3 cm, then will spread to the surface water and sediment surface wood grain brick, brick face gently with wooden hammer knock wood grain brick, until smooth level off, on line and tidy.
Step 8: "brick"
The shop is stuck to pay attention to wood grain brick texture sequence, look for the wood grain brick tile bottom labeled arrows, etc., avoid empty hammer knock wood, balancing power, hard to avoid is too large or too small.The best application tiles with plastic cross, so that we can better locate for wood grain brick.Wooden hammer knock wood grain brick seam anti overflow slurry with sponge or cloth can be erased.High-grade wood grain brick generally gap less than 1 mm, do not need special caulking.
Step 9: "nap"
Lay good wood grain brick, cement is not completely dry, can be observed with the naked eye or with level measurement, according to the standard for finishing wood grain brick.Check the brick pavement smoothness, straightness brick joints, etc.Found the problem, immediately, serious pry wood grain brick shop is stuck again.
Step 10: caulking
After waiting for cement dry to gap filling in with iron hook jointing, combined with tie-in color caulking agent caulking.
This paper provided by okorder:
http://www.okorder.com/bricks_pl36136.html
Related to share:
https://plus.google.com/118350281165358888682/posts/ACcbktkRocG
https://plus.google.com/118350281165358888682/posts/MoWWX1vo1NL
https://plus.google.com/118350281165358888682/posts/Ui6XYksB37i